Car seat series
Note: The parameters are for reference only. We will customize functional leather fabrics according to user needs.
ITEM | Product Data/Parameters For Each Series | |
---|---|---|
Microfiber Leather | Solvent-Free PU | |
Width | 1.0-1.4mm | Warp:≥450N/3CM Went::≥250N/3CM |
Thickness | 52-54" | |
Elongation at break | J:20% W30% | Warp:≥75%/3CM Went::≥50%/3CM |
Peel strength | J:8kg W:8kg | Warp:≥50N/3CM Went::≥50N/3CM |
Tear strength | J:14kg W:13kg | Warp:≥40N/3CM Went::≥35N/3CM |
Flexibility | Room temperature: 50,000 times | Normal Atmospher ic Temperature:≥400000/Times Minus 20°C:≥100000/Times |
Color fastness to friction | Dry wiping: Level 4 Wet wiping: Level 4 | Dray Rub:4-5 Level Wet Rub:4-5 Level |
Abrasion resistance | 5000 rpm without damage | Martindale:≥100000 times Taber Standard:≥2000 times |
Hydrolysis resistance | 5 years hydrolysis resistance | 10%(m/m)NaOH Solution:≥192h No sense of lubr ication |
Puncture resistance | ≥90N | |
Yellowing resistance | Level 4 | ≥4 Level |
Car dashboard
ITEM | Product Data/Parameters For Each Series | |
---|---|---|
Microfiber Leather | Solvent-Free PU | |
Width | 1.0-1.4mm | Warp:≥450N/3CM Went::≥250N/3CM |
Thickness | 52-54" | |
Elongation at break | J:20% W30% | Warp:≥75%/3CM Went::≥50%/3CM |
Peel strength | J:8.5kg W:7kg | Warp:≥50N/3CM Went::≥50N/3CM |
Tear strength | J:14kg W:13kg | Warp:≥40N/3CM Went::≥35N/3CM |
Flexibility | Room temperature: 50,000 times | Normal Atmospher ic Temperature:≥400000/Times Minus 20°C:≥100000/Times |
Color fastness to friction | Dry wiping: Level 4 Wet wiping: Level 4 | Dray Rub:4-5 Level Wet Rub:4-5 Level |
Abrasion resistance | 5000 rpm without damage | Martindale:≥100000 times Taber Standard:≥2000 times |
Hydrolysis resistance | 5 years hydrolysis resistance | 10%(m/m)NaOH Solution:≥192h No sense of lubr ication |
Puncture resistance | ≥90N | |
Yellowing resistance | Level 4 | ≥4 Level |
Automobile interior panels
ITEM | Product Data/Parameters For Each Series | |
---|---|---|
Microfiber Leather | Solvent-Free PU | |
Width | 0.5-1.4mm | Warp:≥450N/3CM Went::≥250N/3CM |
Thickness | 52-54" | |
Elongation at break | J:20% W35% | Warp:≥75%/3CM Went::≥50%/3CM |
Peel strength | (3cm)J:7kg W:6.5kg | Warp:≥50N/3CM Went::≥50N/3CM |
Tear strength | J:6kg W:5kg | Warp:≥40N/3CM Went::≥35N/3CM |
Flexibility | Room temperature: 30,000 times | Normal Atmospher ic Temperature:≥400000/Times Minus 20°C:≥100000/Times |
Color fastness to friction | Dry wiping: Level 4 Wet wiping: Level 4 | Dray Rub:4-5 Level Wet Rub:4-5 Level |
Abrasion resistance | 2000 rpm without damage | Martindale:≥100000 times Taber Standard:≥2000 times |
Hydrolysis resistance | 5 years | 10%(m/m)NaOH Solution:≥192h No sense of lubr ication |
Puncture resistance | ≥90N | |
Yellowing resistance | Level 4 | ≥4 Level |